1 results listed
In the stand pipes, which are the only evacuation point of
the raw gas released during the high temperature coking of the
coal, the section reduction occurs due to the carbonization and the
problem of degazing of the raw coke gas is experienced. This leads
to an increase in the internal pressure of the raw gas in the furnace
and emissions to the doors, which are the weakest points for sealing.
It also leads to energy losses depending on the amount of leakage.
The raw gas passing through the vertical chimneys is 900 degrees
and it is isolated with fireclay bricks to protect the metal parts. In
this improvement, high-alumina castable mortar is used instead of
fireclay bricks. This has resulted in a reduction in emissions and
maintenance costs.
International Conference on Advanced Technologies, Computer Engineering and Science
ICATCES
Adnan NEHROZOĞLU
Erdal ÜNAL
Bülent ÖZTÜRK
Murat YAMAN
Ozan TURHAN